Plastic mold design elements
The first decision in any plastic mould design is how the finished part is divided between the cavity and the core. The cavity forms the external surfaces and the core forms the internal ones, but the split is not simply a matter of choosing the larger volume for the cavity. It has to satisfy three requirements at once: the parting line must fall on a surface of the part where a small witness mark is acceptable, the two halves must be rigid enough to carry the pressure of the material, and the design must permit the part to be released without distortion.
For a simple drawn cup the core is the male form and the cavity is the female form, so the parting line sits on the rim. For an open tray the split usually occurs at the flange, with the core carrying the drawn wall. Where a part has a snap feature, a slide or a side core, the split has to be arranged so that those features are not undercut by the draw direction of the main tool halves.
The parting line is the single most visible quality characteristic of a moulded part. A well chosen line is invisible, sits flat and follows a surface that can be trimmed or simply accepted. A poor line is visible on every part and, in a visible assembly, is the first thing a customer notices.
Practical guidance is to place the line where the geometry naturally changes, such as the top edge of a flange, the base of a rib, or the transition between a wall and a face. A line placed across a large flat cosmetic surface, or diagonally across a rounded corner, produces a step that cannot be concealed and will usually require a hand operation to remove.
Where the part geometry leaves no obvious location, the line can be placed slightly outside the visible contour so that the flash falls on a surface that is trimmed, or the mould can be built with a shut-off that produces a sub-micron step which is acceptable in most assembly situations.
Draft is the angle applied to surfaces that must release from the mould. Without sufficient draft, a part will either remain in the cavity or be pulled out of the core, and in both cases the risk is damage to the tool rather than simply a poor part.
General practice is a draft of one degree on cores and one and a half degrees on cavities for most textured surfaces, increasing to three degrees on deep or highly polished surfaces. Texturing requires more draft than a polished finish, because the peaks of the texture resist release more strongly than a smooth surface, and a polished cavity that is even slightly under-drafted will show drag marks.
Surface finish is specified as a SPI or equivalent value and is achieved by machining the cavity and then applying the texture with an approved process. The finish specified for the cavity is usually slightly better than the finish specified on the part, because the moulding process adds a small amount of roughness to the surface that is reproduced.
The gate is the point at which material enters the cavity, and its position and size determine the fill pattern, the cosmetic quality at the gate area, and the amount of post-melt material that has to be removed.
The gate should be placed on a surface that will be trimmed, and it should be positioned so that the melt front advances evenly from the gate outward. A gate at one end of a long flat part produces a weld line at the far end where the two melt fronts meet, and that weld line is a visible and mechanically weaker feature. Where a long part must be gated at one point, the design should be adjusted to a geometry that supports an even flow, or a multi-point gate or a hot runner should be considered.
The runner system should be sized so that it does not cool prematurely before the cavity is filled, while not being so large that unnecessary material and cycle time are consumed. Balance is the objective: the pressure drop along the runner should not exceed the pressure drop along the cavity, otherwise the cavity fills at a lower pressure than intended and the part will show short shots or uneven packing.
Cooling determines cycle time more often than any other single factor, and it also determines dimensional stability. The circuit should be laid out as close to the cavity wall as the steel allows, with a consistent distance from the surface so that the cooling rate is uniform around the cavity. A circuit that is too far from the wall extends the cycle, and a circuit that follows an irregular path creates local hot spots and therefore local shrinkage differences.
For a thick section, a baffle or a bubbler is used to bring coolant closer to the centre of the mass. For a deep core, a bubbler is generally more effective than drilling a long channel, because the cooling effect follows the shape of the cavity rather than the geometry of the tool steel. Where a cosmetic surface is critical, the circuit should be arranged so that it does not run directly beneath it, since cooling right under a polished area leaves a visible witness.
The ejection system must release the part from the core without marking the visible surface and without loading the thin sections of the part. The number and position of ejector pins are determined by the part geometry, and the usual rule is to place ejectors on internal or hidden surfaces wherever possible.
Large flat parts tend to distort on cooling, and if the ejectors are concentrated in one area the part is pushed off centre as it is released. In that case ejector pins should be distributed to balance the ejection force, and a stripper plate can be used to keep the part square while the pins move.
Before a design is released for tooling it should pass through a structured review. The questions that catch the largest number of problems are whether the wall thickness is uniform or whether the transition is gradual, whether the part can be released from both halves without undercut, whether the gate and the parting line can be trimmed within the available process, and whether the design allows adequate cooling in the thickest section.
Shrinkage is also a design question rather than a mould room question. A material that shrinks unevenly because of varying wall thickness will produce a part that cannot be assembled, and the correct response is to even out the wall rather than to compensate in the tool. A review at this stage is also the point at which the number of cavities, the target cycle time and the expected tool life should be agreed, since these decisions drive the cost of the tool.